Use of Sustainable Antimicrobial Aggregates for the In-Situ Inhibition of Biogenic Corrosion on Concrete Sewer Pipes.

MRS Advances ◽  
2019 ◽  
Vol 4 (54) ◽  
pp. 2939-2949 ◽  
Author(s):  
Ismael Justo-Reinoso ◽  
Mark T. Hernandez

ABSTRACTA new generation of cementitious materials is being engineered to selectively inhibit the growth of Acidithiobacillus, which are a key genera of acid-generating bacteria responsible for microbially induced concrete corrosion (MICC). In this context, the substitution of metal-laden granular activated carbon (GAC) particles and/or steel slag for a fraction of the fine aggregates traditionally used in concrete mixture has proven useful. While the antimicrobial properties of specific heavy metals (i.e. copper and cobalt) have been leveraged to inhibit acid-generating bacteria growth on sewer pipes, few studies have researched how biocidal aggregates may affect the microstructural and mechanical properties of cementitious materials. We report here on the effects that these biocidal aggregates substitutions can have on compressive strength, flowability, and setting times of cement-based formulations. Results showed that increases in compressive strength, regardless of the presence or absence of biocidal metals, resulted from the GAC incorporation where sand replacement was 3% by mass or lower, while flowability decreased when percentages higher than 3% of GAC was incorporated in a cement mix. When substituting fine aggregate with steel slag particles in mass ratios between 5% and 40%, compressive strength was not affected, regardless of the presence or absence of copper. Setting times were not affected by the inclusion of GAC or steel slag particles except when substituting GAC particles at 10% of the fine aggregate mass; under this condition both initial and final setting times were decreased. Results suggest that in order to have enhanced inhibition potential against acidophilic microorganisms and equal or improved mechanical properties, a combination of 1% metal-laden GAC and 40% copper-laden steel slag is an optimum fine aggregate substitution scenario.

2011 ◽  
Vol 311-313 ◽  
pp. 1949-1952 ◽  
Author(s):  
Ying Li Gao ◽  
Ling Cheng

Cement based composite cementitious material containing steel slag used in road has been prepared to deal with the current situation that the transportation carbon emission increased year by year. In this material, 40% cement has been replaced by equivalent steel slag, which has the ability of CO2sequestration. This paper studied the CO2sequestration effect and the mechanical properties of the pure cement, the pure steel slag, and the cement based composite cementitious materials containing steel slag. It has been shown that the cement based composite cementitious materials containing steel slag have excellent CO2sequestration property. The mass fraction growth rate of carbon reached 10.86% after 1 hour carbonation experiment, the value between which of pure cement and pure steel slag, and the compressive strength of the composite cementitious materials at 28-day age can reach 45.3MPa, meeting the requirements of road.


Materials ◽  
2019 ◽  
Vol 12 (23) ◽  
pp. 3849 ◽  
Author(s):  
Manuel J. Chinchillas-Chinchillas ◽  
Manuel J. Pellegrini-Cervantes ◽  
Andrés Castro-Beltrán ◽  
Margarita Rodríguez-Rodríguez ◽  
Víctor M. Orozco-Carmona ◽  
...  

Currently it is necessary to find alternatives towards a sustainable construction, in order to optimize the management of natural resources. Thus, using recycled fine aggregate (RFA) is a viable recycling option for the production of new cementitious materials. In addition, the use of polymeric microfibers would cause an increase in the properties of these materials. In this work, mortars were studied with 25% of RFA and an addition of polyacrylonitrile PAN microfibers of 0.05% in cement weight. The microfibers were obtained by the electrospinning method, which had an average diameter of 1.024 µm and were separated by means of a homogenizer to be added to the mortar. Cementing materials under study were evaluated for compressive strength, flexural strength, total porosity, effective porosity and capillary absorption, resistance to water penetration, sorptivity and carbonation. The results showed that using 25% of RFA causes decreases mechanical properties and durability, but adding PAN microfibers in 0.05% caused an increase of 2.9% and 30.8% of compressive strength and flexural strength respectively (with respect to the reference sample); a decrease in total porosity of 5.8% and effective porosity of 7.4%; and significant decreases in capillary absorption (approximately 23.3%), resistance to water penetration (25%) and carbonation (14.3% after 28 days of exposure). The results showed that the use of PAN microfibers in recycled mortars allowed it to increase the mechanical properties (because they increase the tensile strength), helped to fill pores or cavities and this causes them to be mortars with greater durability. Therefore, the use of PAN microfibers as a reinforcement in recycled cementitious materials would be a viable option to increase their applications.


2020 ◽  
Vol 27 (3) ◽  
pp. 45-60
Author(s):  
Muataz Nayel ◽  
Ammar Khazaal ◽  
Waleed Alabdraba

Recently, the constructions industry begins to make concrete more sustainable, side by side, with making its high performance. This paper aims to investigate the effect of (Metakaolin and Micro Silica) when they replace cement by (8, 12 and 16) % and (6, 9 and 12) % respectively, recycled steel slag when replaces fine aggregate by (10, 20 and 30) %, and recycled mosaic tiles when replaces coarse aggregate by (33.33, 66.67 and 100) % each one another on the slump, density, absorption and compressive strength of concrete. The experimental results showed that the maximum reduction ratio of cement reach (17%) (8% of metakaolin and 9% Micro Silica) while the optimum percentage of mosaic tiles and steel slag is (100%) and (20%) respectively. The optimum percentages obtained are combining to produce three basic green mixes: 1) 17% (8% of Metakaolin and 9% of Micro Silica) only, (2) A mix containing 17% of (Metakaolin and of Micro Silica) plus 100% of recycled mosaic, (3) 17% of (Metakaolin and Micro Silica), 100% of recycled mosaic and 20% of slag. Compressive strength at (7, 28, and 60) days, modulus of rupture at (28) days, absorption, fresh and hardened density are investigated. The best improvement in compressive strength compared with reference concrete was recorded (20.06, 10.855 and 9.983) % at (7, 28 and 60) days respectively for the mix containing (17% of cementitious materials plus 100% of recycled mosaic) while the ultimate flexure strength (24) % appeared in green mix containing (17% of cementitious materials, 100% of recycled mosaic and 20% of slag). Generally, an inverse relationship between density and absorption in all trail mixes which are conducted


2019 ◽  
Vol 9 (2) ◽  
pp. 195-200 ◽  
Author(s):  
Ghania Sebki ◽  
Brahim Safi ◽  
Kahina Chahour

Abstract This work aims to study the possibility recycling of foundry sand wastes (FSW) as a cementations additive and fine aggregate in self-compacting mortars (SCM). For this, an experimental study was carried out to evaluate physical and mechanical properties of SCM. Firstly, sand is substituted by the foundry sand waste at dosages (0%, 10%, 30%, and 50%) by weight of the sand. Secondly cement is partially substituted by crushed foundry sand waste at different ratio (0%, 10%, 20%, 30%, and 50%) by weight of cement. The obtained results show that up to 50%, (FSW) can be used as fine aggregate for mortars without affecting the essential proprieties of mortar. However, beyond 50% of sand substitution, mortars lose their fluidity. The compressive strength of the mortars with 50% of cement substitution decreased compared to the control mortar. Value of the highest compressive strength recorded at 28 days, is of the order of 50 MPa for the mortar with 20% of cement substitution. Also, stress-strain curve show an acceptable mechanical behavior of FSW-based mortar at 50% of sand substitution.


2019 ◽  
Vol 8 (4) ◽  
pp. 8336-8342

From decades it has been recognized that Geopolymer will considerably replace the role of cement in the construction industry. In general, Geopolymer exhibits the property of the peak compressive strength, minimal creep and shrinkage. In this current research paper, Geopolymer mortar is prepared by using GGBS and Fly ash. The mix proportions are of (100-60)%GGBS with Fly ash by 10% replacement. The alkali activators Na0H and Na2Sio3 are used in the study for two different molarities of 4&8. The ratio to Sodium silicates to sodium hydroxide is maintained from 1.5, 2, 2.5 & 3 were used. Mortars are prepared and studied the effect of molarities of alkali activators in their setting times and strengths


Materials ◽  
2019 ◽  
Vol 12 (23) ◽  
pp. 3927
Author(s):  
Anja Weidner ◽  
Yvonne Ranglack-Klemm ◽  
Tilo Zienert ◽  
Christos G. Aneziris ◽  
Horst Biermann

The present study provides the mechanical properties of a new generation of refractory composites based on coarse-grained Al2O3 ceramic and the refractory metals Nb and Ta. The materials were manufactured by refractory castable technology and subsequently sintered at 1600 °C for 4 h. The mechanical properties and the damage behavior of the coarse-grained refractory composites were investigated at high temperatures between 1300 and 1500 °C. The compressive strength is given as a function of temperature for materials with two different volume fractions of the refractory metals Ta and Nb. It is demonstrated that these refractory composites do not fail in a completely brittle manner in the studied temperature range. The compressive strength for all materials significantly decreases with increasing temperature. Failure occurred due to the formation of cracks along the ceramic/metal interfaces of the coarse-grained Al2O3 particles. In microstructural observations of sintered specimens, the formation of tantalates, as well as niobium oxides, were observed. The lower compressive strength of coarse-grained Nb-Al2O3 refractory composites compared to Ta-Al2O3 is probably attributed to the formation of niobium oxides. The formation of tantalates, however, seems to have no detrimental effect on compressive strength.


2019 ◽  
Vol 12 (1) ◽  
pp. 31-38 ◽  
Author(s):  
N. SCHWANTES-CEZARIO ◽  
M. F. PORTO ◽  
G. F. B. SANDOVAL ◽  
G. F. N. NOGUEIRA ◽  
A. F. COUTO ◽  
...  

Abstract This study aims to evaluate the influence of B. subtilis AP91 spores addition on the mechanical properties of mortars. B. subtilis strain AP91, isolated from rice leaves of the needle variety, which has an early cycle of production, was used at the concentration of 105 spores/mL in mortars with cement-to-sand ratio of 1:3 (by weight) and water-to-cement ratio (w/c) of 0.63. These spores were added in two different ways: in the mixing water and by immersion in a solution containing bacterial spores. Scanning Electron Microscope (SEM) analysis showed crystals with calcium peaks on the EDS, which possibly indicates the presence of bioprecipitated calcium carbonate. The results obtained in the mechanical analysis showed that the bioprecipitation of CaCO3 by B. subtilis strain AP91 was satisfactory, particularly when the spores were added in the mixing water, increasing the compressive strength up to 31%. Thus, it was concluded that the addition of B. subtilis AP91 spores in the mixing water of cement mortars induced biocementation, which increased the compressive strength. This bioprecipitation of calcium carbonate may very well have other advantageous consequences, such as the closure of pores and cracks in cementitious materials that could improve durability properties, although more research is still needed on this matter.


Author(s):  
Moein Khoshroo ◽  
Ali Akbar Shirzadi Javid ◽  
Nima Rajabi Bakhshandeh ◽  
Mohamad Shalchiyan

In this study, the effect of using crumb rubber and recycled aggregates on the mechanical properties of concrete has been evaluated as areplacement of fine and coarse aggregates In order to add the admixtures and evaluate their combined effect, 20 different types of concrete mixture ratio were prepared. The results indicated that in those samples containing crumb rubber and recycled aggregates the compressive strength is reduced and adding fiber up to 0.1%. to these concrete samples can improve the compressive strength Also, the tensile strength of the samples mixed with crumb rubber and recycled aggregates were decreased, and with the addition of propylene fiber up to 0.4%. the tensile strength slightly increased Moreover by adding the crumb rubber to the samples the elasticity modulus was reduced but by adding fiber to samples about 0.1% and 0.2.% the modulus of elasticity of concrete in all samples were increased. According to the results, it can be said that using the combination of 5% of crumb rubber as a replacement of fine aggregate, and the combination of 35% of recycled aggregates as a replacement of coarse aggregate, and also by adding 0.1% polypropylene fiber in volumetric percentage of concrete along with adding 7% of micro silica as a replacement of cement led to the best effect on the mechanical properties of concrete.


2020 ◽  
Vol 833 ◽  
pp. 228-232
Author(s):  
Md. Jihad Miah ◽  
Mohammad Shamim Miah ◽  
Anisa Sultana ◽  
Taukir Ahmed Shamim ◽  
Md Ashraful Alom

This work performs experimental investigations on concrete made with difference replacement percentage of first-class burnt clay brick aggregate (0, 10, 20, 30, 40, 50, 60, 80, and 100%) by steel slag (SS) aggregate. The aim is to evaluate the mechanical properties as well as durability performances, additionally, water absorption porosity test is performed to investigate the influence of steel slag aggregate on the durability of tested concrete. The experimental results have shown that the compressive strength was improved significantly due to the replacement of brick aggregate by steel slag aggregate. The crushing strength of concrete made with 100% steel slag aggregate has gained up to 70% more than the control concrete (100% brick aggregate). However, the porosity of concrete was reduced with the adding percentage of brick aggregate by steel slag aggregate which is consistent with the compressive strength results. Further, a quite good agreement between compressive strength and porosity was observed as well.


Sign in / Sign up

Export Citation Format

Share Document