scholarly journals STUDI PERBANDINGAN SIFAT MEKANIK SERAT BAMBU

Author(s):  
Gregoria Illya ◽  
Ika Bali

Natural fibers have application in almost every item used in our daily routine and been contributing explicitly to the economic prosperity and sustainability in our lives. Among the natural fiber plants, bamboo is the most popular, because of its versatile applications and significant contribution to the environment. Bamboo fibers have been used in various application such as decoration, weaving, paper makin, textile, and high-performance composites for the past many years. They have several advantages such as superior tensile strength, low density, and high flexibility under flexible and compressive loads. In order to meet the requirements of each bamboo application, there is a need to study the mechanical properties of bamboo fibers. This study reviews mechanical properties of bamboo fibers for various species, extraction methods, plant age, sizes, and moisture contents.  Keywords: bamboo fiber; bamboo extraction method; mechanical properties; mechanical testing; tensile strength AbstrakIndonesia kaya akan tanaman yang dapat diambil seratnya untuk diolah menjadi produk yang bermanfaat. Di antara tanaman penghasil serat alami, bambu adalah yang paling populer, karena memiliki aplikasi yang serba guna, mudah tumbuh, tidak memerlukan perawatan dan dapat mengurangi pencemaran udara. Serat bambu telah digunakan dalam berbagai aplikasi seperti dekorasi, perabot, tekstil, kertas dan komposit. Beberapa keunggulan serat bambu adalah memiliki kekuatan tarik yang besar, densitas yang rendah dan fleksibilitas yang tinggi. Dalam rangka memenuhi persyaratan masing-masing aplikasi dari serat bambu, diperlukan studi mengenai sifat mekanik serat bambu. Penelitian ini membandingkan beberapa penelitian yang sudah dilakukan mengenai sifat mekanik serat bambu berdasarkan spesies, metode pengolahan dari batang bambu menjadi serat, umur tanaman, ukuran serat dan kadar kelembaban. Serat bambu yang dihasilkan dapat memiliki sifat mekanik yang optimal jika bambu yang dipilih adalah dari spesies tertentu, memiliki kadar kelembaban yang rendah dan menggunakan metode ekstraksi yang tepat.

Author(s):  
Mohammed Khazal ◽  
Salman H. Abbas ◽  
Younis M. Younis ◽  
Thabit Jamel

This study aims to enhance the mechanical properties of polymer material using type of natural fiber. Bamboo fiber considered the strongest between the natural fibers group, it have low density, high mechanical strength in addition to its availability makes it economically viable and have potential for used as engineering material. The study is concerned with evaluate some of the mechanical properties (Tensile strength, Bending strength, Impact strength) for the resultant composite reinforced with 10, 20 and 30 vol.% of bamboo fibers, as compared with received material. With the natural reinforcement, the optimum mechanical properties in comparison with the as received epoxy were achieved. The results indicated that the tensile strength increased from 13.51 MPa to 33.50 MPa (that is a percentage increase of 150 %), also the bending strength increased from 24.25 MPa to 44.5 MPa (that is a percentage increase about 83 %), as well as, the increase of the impact strength from 41 kJ/m2 to 69 kJ/m2 (that is a percentage increase about 68 %).


2020 ◽  
Vol 8 (6) ◽  
pp. 5393-5397

In the present era, Natural fibers are favored for the formation of composites due to their low density, high strength, biodegradability, easy production, low carbon foot, environment friendly nature in comparison of synthetic fibers. This Paper deals with NFRC made from natural fibers obtained from the plants of arid region of Western Rajasthan on which a few researchers are focusing. This paper discuss on the extraction process of fiber from the ber’s stems, manufacturing of composites by using epoxy resin & ber’s fibers then testing of its mechanical properties e.g. tensile strength, young modulus, yield strength , and percentage elongation. Six Sample were made having weight ratio - 0.1, 0.2, 0.3, 0.4, 0.45, & 0. 6. Dog bone samples were prepared according to the ASTM D638 (Type IV) standard. Tensile strength varies from 12.19 MPa to 25 MPa, while young modulus varies from 1.4GPa to 2.9GPa for different weight ratios. Yield strength varies from 10.77 MPa to 21.16 MPa. Percentage of Elongation varies from 1 to 3%. These results shows that ber’s stems can be used for fiber extraction to manufacture composites materials & for better mechanical properties minimum fiber volume fraction percentage is 13% and maximum fiber fraction is 31%.This data can be used further when optimum value of fiber volume fraction is required to form composites from ber’s fibers.


2017 ◽  
Vol 47 (8) ◽  
pp. 2050-2073 ◽  
Author(s):  
A Praveen Kumar ◽  
M Nalla Mohamed

Economic and environmental concerns lead the researchers toward development of sustainable and renewable materials of which reinforced composites are part of. The abundantly available natural fibers have attracted the researchers to study their performance as reinforcements and feasibility for making automobile components. The performance of composite materials is mainly assessed through their mechanical properties. However, natural fibers to date were mainly used as reinforcements to create bulk composite components with reduced cost rather than improved mechanical performances. Among the methods available for improving mechanical properties of the natural fiber composites, combined mercerization treatment, hybridization, and incorporation of fly ash fillers in the matrix are the best solutions. Therefore, the objective of this research is to evaluate the tensile properties of hybrid kenaf/glass composites with and without fly ash particulate filler as per ASTM standards. Moisture absorption behavior and its effect on the tensile properties of hybrid composites are also investigated. The results revealed that the addition of 10wt % fly ash particles with natural fiber composites increased the tensile strength of composites while hybridization with glass fibers reduced the water absorption properties.


2014 ◽  
Vol 592-594 ◽  
pp. 202-205
Author(s):  
V. Santhanam ◽  
M. Chandrasekaran ◽  
N. Venkateshwaran

Composite materials are widely used for their superior properties such as high strength to weight ratio, high tensile strength, low thermal expansion, low density etc. Due to environmental issues the eco-friendly composites are being explored. Natural fibers as reinforcement for polymer composites are widely studied. But natural fibers lack better mechanical properties when compared with synthetic fibers. Hence mixing the natural fiber with a synthetic fiber such as glass fiber will improve mechanical properties of the composites. In this study banana fiber is mixed with glass fiber, and the mixture is used as reinforcement in epoxy matrix. The composite specimens were prepared using hand layup technique, the fibers were randomly oriented. Further the fiber length was varied as 10, 15, 20 and 25mm and volume fraction as 10%, 15%, 20% and 25%. Experiments were conducted to find the effect of fiber length and volume fraction on tensile strength, flexural strength, water absorption properties of the composites. It is observed that a fiber length of 20mm and 20% fiber volume fraction gave better mechanical properties.


2021 ◽  
Vol 11 (3) ◽  
pp. 177-189
Author(s):  
Irwan Suriaman ◽  
Jooned Hendrarsakti ◽  
Yati Mardiyati ◽  
Ari Darmawan Pasek

In line with economic growth, material requirements in the industrial sector will increase. Industries are required to use materials that are safe for human health, environmentally friendly and utilize local raw materials. Currently, industries in general still use synthetic materials based on petroleum residues that contain many hazardous chemicals. Therefore, natural fiber has the potential to be used as a substitute for synthetic materials, especially in Indonesia which is rich in natural fibers resources. This will have an impact on the socio-economy of the local community so that it can grow the rural economic sector. Natural fibers have high economic value that can be used for various raw material needs for strategic industries. A good natural fiber processing mechanism will produce products that can be marketed globally with guaranteed product quality. This research analyzes the effect of alkali treatment of ramie, sugar palm and coir fiber on the increase in mechanical properties of the fiber. The mechanical properties were analyzed through tensile strength testing of single fiber according to ASTM D3822 standard using a textechno favigraph machine. In addition, this research is supported by data from thermogravimetric analysis (TGA), Fourier-transform infrared spectroscopy (FTIR), and scanning electron microscopy (SEM). The results showed that the fibers that had been given an alkali treatment had better mechanical properties compared to untreated fibers. Increased tensile strength of fibers was observec after being treated with alkali for ramie 81%, sugar palm 52% and coir 56%. The advantage of this alkaline treatment method is that no heating is involved and the treatment procedures are more practical compared to other methods.


2012 ◽  
Vol 85 (1) ◽  
pp. 120-131 ◽  
Author(s):  
Md. Najib Alam ◽  
Swapan Kumar Mandal ◽  
Subhas Chandra Debnath

Abstract Several zinc dithiocarbamates (ZDCs) as accelerator derived from safe amine has been exclusively studied in the presence of thiazole-based accelerators to introduce safe dithiocarbamate in the vulcanization of natural rubber. Comparison has been made between conventional unsafe zinc dimethyldithiocarbamate (ZDMC) with safe novel ZDC combined with thizole-based accelerators in the light of mechanical properties. The study reveals that thiuram disulfide and 2-mercaptobenzothiazole (MBT) are always formed from the reaction either between ZDC and dibenzothiazyledisulfide (MBTS) or between ZDC and N-cyclohexyl-2-benzothiazole sulfenamide (CBS). It has been conclusively proved that MBT generated from MBTS or CBS reacts with ZDC and produces tetramethylthiuram disulfide. The observed synergistic activity has been discussed based on the cure and physical data and explained through the results based on high-performance liquid chromatography and a reaction mechanism. Synergistic activity is observed in all binary systems studied. The highest tensile strength is observed in the zinc (N-benzyl piperazino) dithiocarbamate-accelerated system at 3:6 mM ratios. In respect of tensile strength and modulus value, unsafe ZDMC can be successfully replaced by safe ZDCs in combination with thiazole group containing accelerator.


2021 ◽  
Vol 11 (1) ◽  
Author(s):  
Taslima Ahmed Tamanna ◽  
Shah Alimuzzaman Belal ◽  
Mohammad Abul Hasan Shibly ◽  
Ayub Nabi Khan

AbstractThis study deals with the determination of new natural fibers extracted from the Corypha taliera fruit (CTF) and its characteristics were reported for the potential alternative of harmful synthetic fiber. The physical, chemical, mechanical, thermal, and morphological characteristics were investigated for CTF fibers. X-ray diffraction and chemical composition characterization ensured a higher amount of cellulose (55.1 wt%) content and crystallinity (62.5%) in the CTF fiber. The FTIR analysis ensured the different functional groups of cellulose, hemicellulose, and lignin present in the fiber. The Scherrer’s equation was used to determine crystallite size 1.45 nm. The mean diameter, specific density, and linear density of the CTF fiber were found (average) 131 μm, 0.86 g/cc, and 43 Tex, respectively. The maximum tensile strength was obtained 53.55 MPa for GL 20 mm and Young’s modulus 572.21 MPa for GL 30 mm. The required energy at break was recorded during the tensile strength experiment from the tensile strength tester and the average values for GL 20 mm and GL 30 mm are 0.05381 J and 0.08968 J, respectively. The thermal analysis ensured the thermal sustainability of CTF fiber up to 230 °C. Entirely the aforementioned outcomes ensured that the new CTF fiber is the expected reinforcement to the fiber-reinforced composite materials.


2021 ◽  
Vol 11 (12) ◽  
pp. 5317
Author(s):  
Rafał Malinowski ◽  
Aneta Raszkowska-Kaczor ◽  
Krzysztof Moraczewski ◽  
Wojciech Głuszewski ◽  
Volodymyr Krasinskyi ◽  
...  

The need for the development of new biodegradable materials and modification of the properties the current ones possess has essentially increased in recent years. The aim of this study was the comparison of changes occurring in poly(ε-caprolactone) (PCL) due to its modification by high-energy electron beam derived from a linear electron accelerator, as well as the addition of natural fibers in the form of cut hemp fibers. Changes to the fibers structure in the obtained composites and the geometrical surface structure of sample fractures with the use of scanning electron microscopy were investigated. Moreover, the mechanical properties were examined, including tensile strength, elongation at break, flexural modulus and impact strength of the modified PCL. It was found that PCL, modified with hemp fibers and/or electron radiation, exhibited enhanced flexural modulus but the elongation at break and impact strength decreased. Depending on the electron radiation dose and the hemp fibers content, tensile strength decreased or increased. It was also found that hemp fibers caused greater changes to the mechanical properties of PCL than electron radiation. The prepared composites exhibited uniform distribution of the dispersed phase in the polymer matrix and adequate adhesion at the interface between the two components.


Polymers ◽  
2021 ◽  
Vol 13 (13) ◽  
pp. 2220
Author(s):  
Zaida Ortega ◽  
Francisco Romero ◽  
Rubén Paz ◽  
Luis Suárez ◽  
Antonio Nizardo Benítez ◽  
...  

This paper compares the mechanical properties of different natural fiber composites produced by rotational molding as a way of waste valorization from campaigns to control invasive plant species in Macaronesia. Rotomolded parts produced with polymeric matrices (polyethylene) and filled with up to 20% by weight of cellulosic fibers obtained from Arundo donax L., Pennisetum setaceum, and Ricinus communis plants were characterized in terms of tensile, flexural, and impact strength. It was found that the sieving of natural fibers allowed for their introduction in higher loadings, from 10 (for un-sieved material) to 20%; fiber size greatly affected the mechanical properties of the final parts, although some combinations were proven not to reduce the mechanical properties of the neat resin. This study is a first approach to the valorization of residues obtained from periodic campaigns of the control of invasive species performed by public authorities, usually at the local level. It is important to highlight that the main objective of this research did not focus on economically profitable activity; instead, it was focused on the reduction of wastes to be disposed from ecosystem maintenance actions and the investment of potential income into preservation policies.


2018 ◽  
Vol 2018 ◽  
pp. 1-11 ◽  
Author(s):  
Chatree Homkhiew ◽  
Surasit Rawangwong ◽  
Worapong Boonchouytan ◽  
Wiriya Thongruang ◽  
Thanate Ratanawilai

The aim of this work is to investigate the effects of rubberwood sawdust (RWS) size and content as well as the ratio of natural rubber (NR)/high-density polyethylene (HDPE) blend on properties of RWS reinforced thermoplastic natural rubber (TPNR) composites. The addition of RWS about 30–50 wt% improved the modulus of the rupture and tensile strength of TPNR composites blending with NR/HDPE ratios of 60/40 and 50/50. TPNR composites reinforced with RWS 80 mesh yielded better tensile strength and modulus of rupture than the composites with RWS 40 mesh. The TPNR/RWS composites with larger HDPE content gave higher tensile, flexural, and Shore hardness properties and thermal stability as well as lower water absorption. The TPNR/RWS composites with larger plastic content were therefore suggested for applications requiring high performance of thermal, physical, and mechanical properties.